Carbon & low-alloy cast steel

GS-25CrNiMo4 (1.6515) chemical composition

Low-alloy cast steel GS-25CrNiMo4 (GS25CrNiMo4)

A Cr-Ni-Mo quenched-and-tempered grade from the withdrawn German cast-steel standards, not carried into EN 10293. The nickel addition improves toughness and hardenability over the CrMo grades; still specified on older drawings.

Designation
GS-25CrNiMo4
Material no.
1.6515
Standard
SEW 515 / DIN 17205
Also known as
GS25CrNiMo4
Family
Carbon & low-alloy cast steel

Chemical composition (mass %)

Elementminmax
CCarbon0.220.29
SiSilicon0.300.60
MnManganese0.601.00
PPhosphorus–0.025
SSulphur–0.025
CrChromium0.801.20
NiNickel0.801.20
MoMolybdenum0.200.30
FeIronremainder

Basis of values: Limits per SEW 515 / DIN 17205.

We cast GS-25CrNiMo4

We sand cast carbon and low-alloy steel to EN 10293, EN 10213 and ASTM A216/A352, heat treat it at the foundry (water, oil or air quench) and, if required, machine it in the group's machine shop in Perama. Each heat is checked by spectrometer; orders ship with an EN 10204 3.1 certificate, with mechanical testing and NDT (UT, MT, PT) as specified.

  • Sand casting at our foundry in Mandra, Attica; centrifugal casting for bushings, sleeves and liners
  • Heat treatment at the foundry (water, oil or air quench); CNC machining in our machine shop in Perama
  • Spectrometer analysis of every heat, mechanical testing and NDT
  • EN 10204 3.1 inspection certificates; ISO 9001 (both plants) and ISO 14001 (foundry) certified

Other grades in this family

← All alloy families

For information only, without warranty: limits per the cited standard or, where stated, typical or house values; ≈ marks a comparable grade, not an equivalent. The current edition of the standard, the purchase order and the drawing govern.

Casting Quote

Send us your drawing.
We respond within 24 hours.

PDF, STEP or DWG — or a sample. A single part or a series: cast, heat treated and machined.

Send your drawing → Quote request form
sales@foundry.gr · +30 210 5550700