Carbon & low-alloy cast steel

GE300 (1.0558) chemical composition

Carbon cast steel GE300 (GS-60)

The highest-strength unalloyed grade of EN 10293, successor to GS-60. Its higher strength suits more heavily stressed and wear-loaded machine parts. Only P and S are specified, and welding needs more care than with GE200 or GE240.

Designation
GE300
Material no.
1.0558
Standard
EN 10293
Also known as
GS-60
Family
Carbon & low-alloy cast steel

Chemical composition (mass %)

Elementminmax
PPhosphorus–0.035
SSulphur–0.03
FeIronremainder

Basis of values: Limits per EN 10293.

We cast GE300

We sand cast carbon and low-alloy steel to EN 10293, EN 10213 and ASTM A216/A352, heat treat it at the foundry (water, oil or air quench) and, if required, machine it in the group's machine shop in Perama. Each heat is checked by spectrometer; orders ship with an EN 10204 3.1 certificate, with mechanical testing and NDT (UT, MT, PT) as specified.

  • Sand casting at our foundry in Mandra, Attica; centrifugal casting for bushings, sleeves and liners
  • Heat treatment at the foundry (water, oil or air quench); CNC machining in our machine shop in Perama
  • Spectrometer analysis of every heat, mechanical testing and NDT
  • EN 10204 3.1 inspection certificates; ISO 9001 (both plants) and ISO 14001 (foundry) certified

Other grades in this family

← All alloy families

For information only, without warranty: limits per the cited standard or, where stated, typical or house values; ≈ marks a comparable grade, not an equivalent. The current edition of the standard, the purchase order and the drawing govern.

Casting Quote

Send us your drawing.
We respond within 24 hours.

PDF, STEP or DWG — or a sample. A single part or a series: cast, heat treated and machined.

Send your drawing → Quote request form
sales@foundry.gr · +30 210 5550700