GX40CrNiSi27-4 (1.4823) chemical composition
Low-nickel, high-chromium ferritic-austenitic heat-resistant cast steel. Suited to oxidising and sulphur-bearing atmospheres in which nickel-rich grades are attacked, but with limited creep strength; typical for grate bars and lightly loaded furnace parts.
- Designation
- GX40CrNiSi27-4
- Material no.
- 1.4823
- Standard
- EN 10295
- Also known as
- ≈ ASTM A297 HC / HD
- Family
- Heat-resistant cast steel
Chemical composition (mass %)
| Element | min | max |
|---|---|---|
| CCarbon | 0.30 | 0.50 |
| SiSilicon | 1.00 | 2.50 |
| MnManganese | – | 1.50 |
| PPhosphorus | – | 0.04 |
| SSulphur | – | 0.03 |
| CrChromium | 25.0 | 28.0 |
| NiNickel | 3.00 | 6.00 |
| MoMolybdenum | – | 0.50 |
| FeIron | remainder | |
Basis of values: Limits per EN 10295.
We cast GX40CrNiSi27-4
We produce heat-resistant castings by sand casting, and by centrifugal casting for cylindrical parts such as rings, bushings and sleeves. Every heat is analysed by OES; heat treatment, CNC machining in the group's Perama machine shop and EN 10204 3.1 certificates are available.
- Sand casting at our foundry in Mandra, Attica; centrifugal casting for bushings, sleeves and liners
- Heat treatment at the foundry (water, oil or air quench); CNC machining in our machine shop in Perama
- Spectrometer analysis of every heat, mechanical testing and NDT
- EN 10204 3.1 inspection certificates; ISO 9001 (both plants) and ISO 14001 (foundry) certified
Other grades in this family