GX25CrNiSi20-14 (1.4832) chemical composition
20Cr-14Ni austenitic heat-resistant cast steel with the lowest carbon range of the EN 10295 Cr-Ni grades listed here. Used for furnace fittings and parts at moderate temperatures where good oxidation resistance at lower alloy cost is sufficient.
- Designation
- GX25CrNiSi20-14
- Material no.
- 1.4832
- Standard
- EN 10295
- Also known as
- ≈ AISI 309 (cast), ≈ 1.4828 (wrought)
- Family
- Heat-resistant cast steel
Chemical composition (mass %)
| Element | min | max |
|---|---|---|
| CCarbon | 0.15 | 0.35 |
| SiSilicon | 0.50 | 2.50 |
| MnManganese | – | 2.00 |
| PPhosphorus | – | 0.04 |
| SSulphur | – | 0.03 |
| CrChromium | 19.0 | 21.0 |
| NiNickel | 13.0 | 15.0 |
| MoMolybdenum | – | 0.50 |
| FeIron | remainder | |
Basis of values: Limits per EN 10295.
We cast GX25CrNiSi20-14
We produce heat-resistant castings by sand casting, and by centrifugal casting for cylindrical parts such as rings, bushings and sleeves. Every heat is analysed by OES; heat treatment, CNC machining in the group's Perama machine shop and EN 10204 3.1 certificates are available.
- Sand casting at our foundry in Mandra, Attica; centrifugal casting for bushings, sleeves and liners
- Heat treatment at the foundry (water, oil or air quench); CNC machining in our machine shop in Perama
- Spectrometer analysis of every heat, mechanical testing and NDT
- EN 10204 3.1 inspection certificates; ISO 9001 (both plants) and ISO 14001 (foundry) certified
Other grades in this family
For information only, without warranty: limits per the cited standard or, where stated, typical or house values; ≈ marks a comparable grade, not an equivalent. The current edition of the standard, the purchase order and the drawing govern.