Heat-resistant cast steel

HT (35Ni-17Cr) chemical composition

Heat-resistant cast steel HT (35Ni-17Cr)

35Ni-17Cr grade in which nickel exceeds chromium, giving good resistance to thermal cycling, thermal shock and carburisation. Typical for heat-treatment fixtures, trays, muffles and carburising-furnace parts.

Designation
HT
Standard
ASTM A297
Also known as
35Ni-17Cr
Family
Heat-resistant cast steel

Chemical composition (mass %)

Elementminmax
CCarbon0.350.75
SiSilicon–2.50
MnManganese–2.00
PPhosphorus–0.04
SSulphur–0.04
CrChromium15.019.0
NiNickel33.037.0
MoMolybdenum–0.50
FeIronremainder

Basis of values: Limits per ASTM A297.

We cast HT

We produce heat-resistant castings by sand casting, and by centrifugal casting for cylindrical parts such as rings, bushings and sleeves. Every heat is analysed by OES; heat treatment, CNC machining in the group's Perama machine shop and EN 10204 3.1 certificates are available.

  • Sand casting at our foundry in Mandra, Attica; centrifugal casting for bushings, sleeves and liners
  • Heat treatment at the foundry (water, oil or air quench); CNC machining in our machine shop in Perama
  • Spectrometer analysis of every heat, mechanical testing and NDT
  • EN 10204 3.1 inspection certificates; ISO 9001 (both plants) and ISO 14001 (foundry) certified

Other grades in this family

← All alloy families

For information only, without warranty: limits per the cited standard or, where stated, typical or house values; ≈ marks a comparable grade, not an equivalent. The current edition of the standard, the purchase order and the drawing govern.

Casting Quote

Send us your drawing.
We respond within 24 hours.

PDF, STEP or DWG — or a sample. A single part or a series: cast, heat treated and machined.

Send your drawing → Quote request form
sales@foundry.gr · +30 210 5550700