Heat-resistant cast steel

GX40CrNiSi25-20 (1.4848) chemical composition

Heat-resistant cast steel GX40CrNiSi25-20 (HK40)

Fully austenitic 25Cr-20Ni heat-resistant cast steel, the 25-20 workhorse of EN 10295. Higher nickel than 1.4837 gives better creep strength and structural stability for furnace rolls, radiant tubes, trays and fixtures.

Designation
GX40CrNiSi25-20
Material no.
1.4848
Standard
EN 10295
Also known as
≈ HK40, 25Cr-20Ni, ≈ 1.4841 / 1.4845 (wrought), G-X40CrNiSi25-20
Family
Heat-resistant cast steel

Chemical composition (mass %)

Elementminmax
CCarbon0.300.50
SiSilicon1.002.50
MnManganese–2.00
PPhosphorus–0.04
SSulphur–0.03
CrChromium24.027.0
NiNickel19.022.0
MoMolybdenum–0.50
FeIronremainder

Basis of values: Limits per EN 10295.

We cast GX40CrNiSi25-20

We produce heat-resistant castings by sand casting, and by centrifugal casting for cylindrical parts such as rings, bushings and sleeves. Every heat is analysed by OES; heat treatment, CNC machining in the group's Perama machine shop and EN 10204 3.1 certificates are available.

  • Sand casting at our foundry in Mandra, Attica; centrifugal casting for bushings, sleeves and liners
  • Heat treatment at the foundry (water, oil or air quench); CNC machining in our machine shop in Perama
  • Spectrometer analysis of every heat, mechanical testing and NDT
  • EN 10204 3.1 inspection certificates; ISO 9001 (both plants) and ISO 14001 (foundry) certified

Other grades in this family

← All alloy families

For information only, without warranty: limits per the cited standard or, where stated, typical or house values; ≈ marks a comparable grade, not an equivalent. The current edition of the standard, the purchase order and the drawing govern.

Casting Quote

Send us your drawing.
We respond within 24 hours.

PDF, STEP or DWG — or a sample. A single part or a series: cast, heat treated and machined.

Send your drawing → Quote request form