EN-GJS-1050-6 (EN 1564) chemical composition

Austempered ductile iron EN-GJS-1050-6 (ADI 1050)

Mid-range ADI combining strength and elongation, alloyed with Ni, Mo and Cu for hardenability, used for gears, crankshafts and structural drivetrain parts replacing forged steel. Typical chemistry; EN 1564 sets no composition.

Designation
EN-GJS-1050-6
Standard
EN 1564
Also known as
ADI 1050
Family
Austempered ductile iron (ADI)

Chemical composition (mass %)

Elementminmax
CCarbon3.403.80
SiSilicon2.202.80
MnManganese0.200.40
PPhosphorus–0.05
SSulphur–0.02
CrChromium–0.10
NiNickel0.502.00
MoMolybdenum0.100.40
CuCopper0.501.00
MgMagnesium0.030.06
FeIronremainder

Basis of values: EN 1564 specifies mechanical properties, not chemistry. The values shown are typical foundry ranges; the chemistry is adjusted so the casting meets the requirements of the ordered grade.

EN-GJS-1050-6: castings on request

Castings in these grades on request — send your drawing and required standard for a feasibility check.

  • Sand casting at our foundry in Mandra, Attica; centrifugal casting for bushings, sleeves and liners
  • Heat treatment at the foundry (water, oil or air quench); CNC machining in our machine shop in Perama
  • Spectrometer analysis of every heat, mechanical testing and NDT
  • EN 10204 3.1 inspection certificates; ISO 9001 (both plants) and ISO 14001 (foundry) certified

Other grades in this family

← All alloy families

For information only, without warranty: limits per the cited standard or, where stated, typical or house values; ≈ marks a comparable grade, not an equivalent. The current edition of the standard, the purchase order and the drawing govern.

Casting Quote

Send us your drawing.
We respond within 24 hours.

PDF, STEP or DWG — or a sample. A single part or a series: cast, heat treated and machined.

Send your drawing → Quote request form
sales@foundry.gr · +30 210 5550700